Temperature dependent electrical resistivity in nanocrystalline gold films made by advanced gas deposition Academic Article uri icon

abstract

  • Nanocrystalline gold films were made by advanced gas deposition. The mean crystallite diameter lay between 10 and 80 nm depending on substrate temperature during deposition and annealing post-treatment, as found by x-ray diffractometry and transmission electron microscopy. Temperature dependent resistivity p was measured in the 4

published proceedings

  • Journal of Applied Physics

author list (cited authors)

  • Ederth, J., Kish, L. B., Olsson, E., & Granqvist, C. G.

citation count

  • 17

complete list of authors

  • Ederth, J||Kish, LB||Olsson, E||Granqvist, CG

publication date

  • December 2000